Dry laminating method | Hot melt bonding method | |
Feature |
|
|
Property |
|
|
Application |
|
|
Product | Type | Solid content (%) | Viscosity (cps/25°C) | Solvent | Application |
DPU-205K | 2-component General ester type | 65±2 | 5,000 - 6,000 | MEK | Industrial use Film, film laminating adhesive |
DPU-218E | 2-component General ester type | 60±2 | 6,000 - 7,000 | TOL, Et-Ac | Abrasive sheet Filler, paper adhesive |
DPU-219 | 2-component General ester type | 75±2 | 6,000 - 7,000 | Et-Ac | Abrasive sheet Filler, paper adhesive |
DPU-7045HM | 1-component Co-polymer Type | 45±2 | 10,000 - 20,000 | DMF, MEK | Smartphone case fabric Plastic adhesive hot-melt |
DPU-717HM | 1-component General ester type | 45±2 | 5,000 - 7,000 | DMF, MEK | Smartphone case fabric Plastic adhesive hot-melt |
DPU-7100HM | 1-component Co-polymer Type | 99.5±0.5 | Solid state / 25℃ 5,000 - 80℃ | - | For attaching electronic materials(circuit boards, etc) Reactive hot-melt |
* TOL : Toluene / Et-Ac : Ethyl Acetate / MEK : Methyl Ethyl Ketone / DMF : Dimethylformamide
Product | Type | Solid content (%) | Viscosity (cps/25°C) | pH | Application |
DP-4040 | Polyvinyl acetate | 40~42 | 6,000~8,000 | 3~5 | For coating the inside of bottle caps with paper |
DP-960 | Polyvinyl acetate | 50~53 | 2,000~5,000 | 4~5 | Cigarette filter paper non-woven fabric (for antimicrobial and moisture-proof purposes) |
DP-940 | Polyvinyl acetate | 39~41 | ≤100 | 3~4 | Emulsifiable pesticides |
DP-510D | Polyvinyl acetate | 49~51 | 10,000~13,000 | 4~5 | Paper adhesive |
주식회사 디에스캠솔 | 대표이사: 이승재
사업자등록번호: 133-81-22884
충청북도 충주시 주덕읍 중원산업로 178
TEL: 043-840-2600 | FAX 043-840-2635
E-mail: dwm@dschemsol.com
Copyright ⓒ 2023 dschemsol All rights reserved.
DS CHEMSOL INC. | CEO: Seungjae Lee | Business Registration Number: 133-81-22884
178 Joongwonsanup-ro, Judeok-eup, Chungju-si, Chungcheongbuk-do, South Korea(27459)